Discussion Starter · #4 ·
Sorry took so long to get back on here,busy week.

I used rust-oleum camouflage for plastics and krylon fusion for the clear coat. 3 coats of each with an overnight wait between coats. So far so good...in and out of a hard and soft holster a bunch of times with very little rub off. I'm very happy for a cheap rattle can job.
 